The welding core is the metal core of the electrode. In order to ensure the quality of the weld, there are strict regulations on the content of various metal elements in the weld core. In particular, there are strict restrictions on harmful impurities (such as sulfur and phosphorus), and the quality of the weld core metal should be better than that of the base metal. Arc welding cannot be carried out on a smooth rod without a coating. This is because the arc stability is very poor, splashing is very large, and the weld is not well formed. After long-term practice, it is gradually found that the performance of the electrode is greatly improved by coating the welding core with some mineral raw materials (i.e. electrode coating). (1) Ensure stable arc combustion, so that the welding process is normal. (2) Using the gas produced after the drug skin reaction, protect the arc and the molten pool, prevent the harmful gases in the air (such as nitrogen, oxygen, etc.) from invading the molten pool, such as these gases will cause cracks and pores in the welding material, so that the welding can not achieve the ideal effect. (3) After the drug skin is melted, slag is formed, which covers the weld surface to protect the weld metal, make the weld metal slowly cool, help the gas escape, prevent the generation of pores, and improve the structure and performance of the weld. (4) After melting, various metallurgical reactions will be carried out, such as deoxygenation, sulfur removal, phosphorus removal, etc., so as to improve weld quality and reduce alloying element burning loss.
Broken wire is the iron bright wire, fire wire, galvanized wire, plastic coated wire, paint wire and other metal wire, wire factory according to customer requirements for straightening after sizing cut, has the characteristics of easy transportation, easy to use, widely used in the construction industry, handicrafts, daily civilian and other fields. No limit on length, packing as required. Annealing wire also known as black oiled wire, black annealing wire, fire wire, black iron wire. Compared with cold drawing, black annealed wire is more economical as raw material for nails.
The welding core is the metal core of the electrode. In order to ensure the quality of the weld, there are strict regulations on the content of various metal elements in the weld core. In particular, there are strict restrictions on harmful impurities (such as sulfur and phosphorus), and the quality of the weld core metal should be better than that of the base metal. Arc welding cannot be carried out on a smooth rod without a coating. This is because the arc stability is very poor, splashing is very large, and the weld is not well formed. After long-term practice, it is gradually found that the performance of the electrode is greatly improved by coating the welding core with some mineral raw materials (i.e. electrode coating). (1) Ensure stable arc combustion, so that the welding process is normal. (2) Using the gas produced after the drug skin reaction, protect the arc and the molten pool, prevent the harmful gases in the air (such as nitrogen, oxygen, etc.) from invading the molten pool, such as these gases will cause cracks and pores in the welding material, so that the welding can not achieve the ideal effect. (3) After the drug skin is melted, slag is formed, which covers the weld surface to protect the weld metal, make the weld metal slowly cool, help the gas escape, prevent the generation of pores, and improve the structure and performance of the weld. (4) After melting, various metallurgical reactions will be carried out, such as deoxygenation, sulfur removal, phosphorus removal, etc., so as to improve weld quality and reduce alloying element burning loss.
Compared with galvanizing, hot-dip galvanizing has lower production cost and less environmental impact than galvanizing. Because the coating obtained is thicker, hot-dip galvanizing has better protective performance than electric galvanizing, so it is an important protective coating for steel parts used in harsh working environment. Hot-dip galvanized products are widely used in chemical equipment, petroleum processing, ocean exploration, metal structure, electric power transmission, shipbuilding and other industries.
Each coil of steel wire shall consist of one wire. The surface of the rod shall not have cracks, folds, scars, ears, layers or inclusions. However, indentation, pits, bumps, scratches and pockmarks are allowed, and the depth or height shall not be 0.2mm. There should be no corrosion and oxidation skin on the surface of the steel wire, and oxidation color is allowed by heat treatment. The surface of the wire is allowed to have scratches not exceeding half of the allowable deviation range of the diameter, and local defects not exceeding the allowable deviation of the appropriate diameter.
Although galvanized iron wire has the protection of galvanized layer, it does not say that it will not rust at all, but delays the time of rust. In general, cold galvanized iron wire can be kept for 1-2 years without rust, hot galvanized iron wire can be used for 8-10 years without rust. If properly maintained, the use time will be longer. So how to prevent galvanized iron wire rust?
Galvanized wire mesh is divided into hot dip galvanized wire mesh and cold galvanized wire mesh. Galvanized steel wire net selects the high quality low carbon steel wire, iron wire factory made by precision of automation machinery welding technology processing, smooth surface, firm structure, integrity is strong, even if the local cutting of galvanized steel wire net, or local also under pressure from loose phenomenon, after molding, wire mesh galvanized corrosion resistance good, has the advantage that the general steel mesh does not have.