Low and medium carbon steel wire is used as raw material, with good surface gloss, uniform zinc layer, strong adhesion, corrosion resistance and so on. Available: diameter 1.60mm-4mm (16#-33#) cold plating wire; Diameter 6.40mm-0.81mm(8#-21#) black iron wire, changed wire. It is mainly used in communication equipment, medical equipment, weaving net, brush, steel cable, filter, high-pressure pipe, construction, crafts and other industries.
Generally, the main reasons for the rust of iron wire are: when the steel mesh in the metal mesh appears some dust, this time you can use some water or alkaline solution cleaning. Followed by floating iron or embedded iron, iron will rust, connected to the stainless steel plate mesh of iron rust, so these iron must be dealt with, can use carbon steel wire brush can also be used for processing carbon steel and so on. Then is the scratch, for the scratch, mainly in the production process, need some stubborn iron scratch stainless steel plate net special polishing cleaning machine.
The surface coating of galvanized wire can be seen whether the quality of galvanized wire is good or not. If the strength of zinc attached to the wire is very poor, then this galvanized wire do not buy, because this galvanized wire must be poor galvanized wire. High quality galvanized wire in general, the zinc layer attached to the surface of the wire is relatively thick, so when we buy galvanized wire, as long as we look at the thickness of the zinc layer, we can generally judge the quality of galvanized wire.